Preparation and property of two kinds of polyester oxygen scavenger material

LIU Liu1,CUI Aijun1,HE Mingyang1,CHEN Qun1,CAI Yuming2   

  1. 1School of Petrochemical Engineering,Changzhou University,Changzhou 213164,Jiangsu,China;
    2Jiangsu Angete New Material Science and Technology Limited Company,Changzhou 213161,Jiangsu,China)
  • Online:2012-02-05 Published:2012-02-05

两类聚酯吸氧材料的制备及性能

刘  柳1,崔爱军1,何明阳1,陈  群1,蔡煜明2   

  1. 1常州大学石油化工学院,江苏 常州 213164;2江苏安格特新材料科技有限公司,江苏 常州 213161)

Abstract: Maleic anhydride/2-butene-1,4-diol and maleic anhydride/terminated polybutadiene oxygen scavenger have been prepared by esterification. The influence of reaction time and ratio of alcohol-anhydride on the esterification rate has been discussed,and maleic anhydride/2-butene-1,4-diol and maleic anhydride/terminated polybutadiene oxygen scavenger have been grafted to PET for preparing oxygen scavenger material. Physical property and oxygen absorption of oxygen scavenger material of 2-butene-1,4-diol and terminated polybutadiene were investigated. Retained ratio of double bonds,catalyst amount,and ratio of alcohol-anhydride were investigated. The results showed the optimal preparation condition of 2-butene-1,4-diol oxygen scavenger reaction time would be 2h under which maleic anhydride esterification rate reached 62.55%,maximum number-average molar mass of 2-butene-1,4-diol oxygen scavenger material reached 36607,retained maximum ratio of double bonds of 2-butene-1,4-diol oxygen scavenger material reached 77.4%,the absorbed oxygen volume of 2-butene-1,4-diol oxygen scavenger material would be 3.17 mL,maximum catalyst amount of 2-butene-1,4-diol oxygen scavenger material and terminated polybutadiene oxygen scavenger material reached 1.0 g/kg. Terminated polybutadiene oxygen scavenger reaction time would be 3h under which maleic anhydride esterification rate reached 59.38%,the absorbed oxygen volume of terminated polybutadiene oxygen scavenger material would be 10.04 mL,maximum number-average molar mass of terminated polybutadiene oxygen scavenger material reached 49735,maximum ratio of double bonds of 2-butene-1,4-diol oxygen scavenger material reached 76.3%.

Key words: 2-butene-1,4-diol, terminated polybutadiene, PET, oxygen scavenger

摘要: 制备了1,4-丁烯二醇/顺丁烯二酸酐和端羟基聚丁二烯(HTPB)/顺丁烯二酸酐酯化物吸氧剂,讨论了反应时间及醇酐比对吸氧剂酯化率的影响,并且将1,4-丁烯二醇/顺酐、HTPB/顺酐吸氧剂接枝共聚到PET中得到改性吸氧材料。考察了两种吸氧材料的物理性能和吸氧性能,以及影响吸氧性能的双键保留率,催化剂用量、醇酐比。实验表明,顺酐与1,4-丁烯二醇、HTPB反应的最佳酯化时间分别为2 h和3 h,含1,4-丁烯二醇/顺酐和HTPB/顺酐的吸氧材料最大数均分子量分别为3.66万和4.97万,最大双键保留率分别为77.4%和76.3%,最大催化剂用量为1.0 g/kg,含1,4-丁烯二醇/顺酐和HTPB/顺酐的吸氧材料24 h最大吸氧量为3.17 mL/g和10.04 mL/g。

关键词: 1,4-丁烯二醇, 端羟基聚丁二烯, 聚对苯二甲酸乙二醇酯, 吸氧剂